What are the requirements for surface protection of stainless steel stamping parts?

  85
Author:Jidong New Materials

The surface protection of stainless steel stamping parts has the following core requirements for protective films:

不锈钢冲压件-5.jpg

1. Key performance requirements

1. Adhesive compatibility

- Use acrylic low-viscosity glue (viscosity value recommended 3-6N/25mm) to ensure that there is no residual glue after stamping, especially for BA surface (mirror/bright surface) stainless steel, silicone-free water must be used.

- Viscosity must be temperature stable: viscosity should not decay in a stamping oil environment (80-120°C).


2. Heat resistance

- Short-term heat resistance must reach **150℃/30min** (simulating continuous stamping heat accumulation), and the peel strength change rate after high temperature must be less than 15%.


3. Material mechanical properties

- The base film thickness is recommended to be ≥50μm (mirror-finished parts) to 80μm (deep-stamped parts), with tensile strength >40MPa and elongation >300% to accommodate deep drawing deformation of more than 5mm.

- The puncture strength must be greater than 20N (simulating the stress concentration at the R corner of the stamping die).


4. Chemical compatibility

- It must pass a 48h salt spray test (5% NaCl) and a 72h acid-base oil test (pH 3-11, including stamping oil environment), and no permeation corrosion should occur on the edge of the protective film.

铝板冲压保护-1.jpg


2. Strengthening requirements in special scenarios

1. Surface treatment adaptation solution

- Mirror surface (BA surface): Optical grade PET substrate with haze <5% and surface roughness Ra≤0.1μm is required.

- Brushed surface: The protective film needs to be slightly elastic (elastic modulus 0.5-1.2GPa) to avoid texture collapse.

- Titanium coating/PVD coating: The protective film must pass the 168h 100-grid test (ASTM D3359 B method).


2. Process connection design

- For scenarios where the continuous die stamping line speed is >30 times/minute, the protective film must have anti-high-speed friction wrinkling properties (friction coefficient <0.3).

- Compatibility with welding process pretreatment: The combustion residue of the protective film must meet the ISO 4042 standard (residual ash <0.1mg/cm²).


20241112

3. Quality Verification Standards

1. Process testing specifications

- Simulated stamping test: Use the actual mold to perform ≥500 consecutive stampings, and the protective film breakage rate must be <0.5%.

- Environmental aging test: After 500h at 85℃/85%RH, the peel strength retention rate is >90%.


2. Traceability and packaging

- The protective film is required to have a readable QR code (in compliance with GS1 standards), and each roll of independent packaging must contain a desiccant (dew point < -40°C).



IV. Demand for value-added services

1. Collaborative process development

- Expect suppliers to provide DOE experimental design to develop special formulas for different materials (such as SUS304/316/430).

- It is recommended to develop smart protective films: with integrated pressure-sensing marks (which can show areas of stamping stress concentration).


2. Environmental compliance

- A complete MSDS report must be provided, which complies with EU REACH (SVHC < 0.1%) and China GB/T 26572 standards.

#stainless steel #protective film

304不锈钢.png