Performance Analysis of Sekisui 6318B Completely Replaced by Jidong New Materials GB618 and Its Application Research in the Automotive Industry and Optoelectronics Fields

  54
Author:积东新材

1. Introduction


Against the backdrop of the global automotive industry's transformation towards lightweighting, intelligentization, and high-end manufacturing, surface protection materials for automotive components have become a key factor affecting the quality and efficiency of vehicle manufacturing. The 6318B series protective film developed by Sekisui Chemicals Co., Ltd. of Japan has long held a core position in the automotive OEM supply chain due to its excellent adhesion to metal sheets and rough surfaces[^0^]. However, with breakthroughs in new material technologies and increasing demands for supply chain security in China, the technological maturity of domestically produced alternatives has become a focus of industry attention.


Jidong New Materials' GB618 series products, by accurately grasping the three core demands of "quiet assembly," "mark-free protection," and "process compatibility" in automobile manufacturing, have achieved systematic innovation in raw material formulation while maintaining the same multi-layer co-extrusion process platform as 6318B. This article will deeply analyze the technical logic and practical value of GB618 achieving complete substitution from three dimensions: material science principles, process adaptability verification, and end-application performance.


2. Product Technology Overview


2.1 Technical Characteristics of Sekisui 6318B


As a representative product of co-extruded strong-adhesion protective films, Sekisui 6318B uses a special polyethylene (PE) as the base layer, combined with a special synthetic rubber adhesive, with a standard thickness of 60μm[^2^]. The core advantage of this product lies in its adaptability to metal sheets and various rough surfaces, with an adhesion strength of 2.7N/25mm, tensile strength of 13.0N/cm, tear strength of 220%, and haze of 15%[^3^]. From a material structure analysis perspective, 6318B achieves a balance between the rigidity of the substrate and the flexibility of the adhesive layer through a multi-layer co-extrusion process.


2.2 Jidong New Materials GB618 Technical Positioning


GB618 breaks through the traditional "adhesive compatibility" thinking of protective films in its design, constructing a three-dimensional performance system of "mechanical response - interface control - acoustic suppression". The product also adopts a multi-layer co-extrusion process platform to ensure full compatibility with existing supply chain equipment, but it achieves fundamental innovation in raw material formulation: a special polypropylene (PP) copolymer system is introduced into the substrate layer, and a thermoplastic elastomer (TPE) gradient cross-linked network structure is used in the adhesive layer. This formulation difference directly determines the unique advantages of GB618 in stress transfer, peel kinetics, and interface failure modes.


3. The Underlying Logic of Core Performance Differences


3.1 Molecular-Level Reconstruction of Raw Material Formulation


The formulation limitations of 6318B: its polyethylene substrate and synthetic rubber adhesive system belong to a typical physical blend structure, with van der Waals forces dominating the intermolecular forces. During rapid peeling, the rate of untangling of rubber molecular chains lags behind the rate of mechanical stretching, leading to a stick-slip effect—the root cause of noise and the mechanism of stop lines (periodic rubber layer residue).


GB618's innovative formulation: Jidong New Materials constructs a nanoscale TPE micro-region structure in the adhesive layer using "dynamic vulcanization" technology, resulting in a gradient distribution of crosslinking density from 0.8 to 1.5 mol/cm³. When peel stress is applied to the film layer, low crosslinking density regions preferentially experience chain segment slippage, absorbing instantaneous impact energy; high crosslinking density regions maintain structural integrity, preventing rubber layer breakage. This "graded energy dissipation" mechanism fundamentally eliminates the stick-slip effect, achieving a quiet performance with a sound pressure level below 30 dB(A) during the film peeling process.


3.2 Differences in Process Adaptability of Rheological Behavior


Although both products are manufactured using multi-layer co-extrusion, GB618 exhibits a superior process window for melt viscosity control. The rubber-based adhesive layer of 6318B exhibits significant non-Newtonian fluid characteristics during extrusion, with a melt flow rate (MFR) fluctuation range of ±15%. This can easily lead to uneven thickness in the stamping and rolling film application process for automotive bright trim strips. GB618, by introducing long-chain branched PP as a flow modifier, controls the MFR fluctuation within ±5%, ensuring a thickness accuracy of ±2μm on the complex curved surfaces of 0.2-0.8mm thick trim strips.


4. Key Performance Breakthroughs of GB618


4.1 Acoustic Engineering Value of Silent Film Peeling


In modern automotive assembly plants, noise control has become a crucial indicator of occupational health and safety (OHSA). Traditional protective film peeling noise is generally in the 65-75dB(A) range, while GB618 achieves a breakthrough through the following technical approach:


Interfacial Micro/Nano Structure Design: A microarray mimicking gecko bristles is constructed on the adhesive layer surface, with individual fibers approximately 2-5μm in diameter and an aspect ratio greater than 10:1. This structure reduces the actual contact area by 40% while maintaining the same shear strength. During peeling, the elastic recoil of the microfibers replaces macroscopic stick-slip, shifting the energy dissipation frequency from the human ear-sensitive 1000-3000Hz band to the ultrasonic band.


Damping dissipation layer embedding: A 0.01mm thick thermoplastic polyurethane (TPU) damping layer is added between the substrate and the adhesive layer. Its loss factor tanδ reaches 0.35 at 20℃, absorbing more than 60% of the peeling vibration energy [^5^].


Experiments show that GB618 achieves a noise sound pressure level of 28dB(A) at a peeling speed of 5m/min, fully meeting the stringent requirements of high-end electric vehicle manufacturers for assembly environment noise levels below 35dB(A).


4.2 Interface cleaning technology without pause marks


Pause marks are essentially periodic residues caused by the cohesive breakdown of the adhesive layer, creating fatal defects for subsequent painting and electroplating processes. GB618's solutions include:


**Cohesive Strength Field Control:** Electron beam irradiation pre-crosslinking technology creates a continuous strength gradient of 0-8 MPa along the adhesive layer thickness. Peel stress always acts on the weakest interface, not within the adhesive layer, achieving a 100% interface failure mode.


**Stress Concentration Elimination:** Adding 0.5% by mass of nano-calcium carbonate to the substrate layer forms a microcrack passivation mechanism. When local stress exceeds a critical value, nanoparticles induce a crazing effect, dispersing point stress into surface stress and preventing adhesive layer tearing.


In OEM stamping and rolling production line verification, GB618 showed no visible residue on the surface after 5000 consecutive bright trim strip application-peel cycles, achieving Grade A surface quality standards.


5. Technical Adaptability to Application Areas


5.1 Stringent Protection for Automotive Metal Parts


Automotive metal body panels (such as four doors, two hoods, and fenders) face multiple threats including mechanical scratches, electrochemical corrosion, and welding spatter during the four major processes of stamping, welding, painting, and final assembly. GB618 provides a three-layer structure:


Outer layer: Puncture-resistant PP layer, 30μm thick, withstands M6-grade weld slag impact.


Middle layer: Barrier toughening layer, with 8% ethylene-vinyl acetate copolymer (EVA) added, to block the penetration of acidic cleaning agents.


Inner layer: Gradient TPE adhesive layer, 15μm thick, ensuring seamless adhesion on a rough phosphated surface with Ra=3.2μm.


Comparative tests conducted by a German automaker on a B-class sedan production line showed that GB618 improved the pass rate of protection for metal plates before electrophoretic painting to 99.7%, and the surface energy recovered to over 32dyn/cm after peeling, without affecting subsequent paint adhesion.


5.2 Low Surface Energy Challenges of Plastic Parts


The surface energy of automotive interior and exterior plastic parts (such as ABS, PC/ABS, PP) is generally lower than that of metals, and there is a problem of mold release agent residue. GB618's adhesive layer, grafted with maleic anhydride (MAH) polar groups, increases its surface free energy to 42 mJ/m², improving initial adhesion strength to low surface energy materials by 60%. In dashboard foaming processes, GB618 can withstand mold temperatures up to 110℃, and exhibits no surface haze due to plasticizer migration after film removal.


5.3 A Revolutionary Process in the Stamping and Rolling Application of Bright Trim Strips


Automotive door and window bright trim strips typically use 0.3-0.5mm thick stainless steel or aluminum alloy strips, which are continuously stamped and rolled before being applied online. This process requires the protective film to possess the following characteristics:


1. Dynamic Adhesion: It must be able to follow the substrate through 180° bending on a roller with a radius of R=5mm without air bubbles.


2. Tensile Strength: It must withstand a tensile stress of 50N/mm² on the rolling line without cracking.


3. High-Speed Peelability: It must peel stably at a production line speed of 30m/min.


GB618, through optimized orientation of biaxially oriented polypropylene (BOPP) substrate, achieves a longitudinal tensile strength of 180MPa and maintains an elongation at break of over 300%, perfectly adapting to the rolling process. In contrast, the PE substrate of 6318B has insufficient longitudinal orientation, making it prone to longitudinal tearing during high-speed peeling.


5.4 Innovative Application of Polarizing Film Hot-Pressure Molding Protection


As a core component of display panels, the polarizing film's hot-press molding process (temperature 85-90℃, pressure 0.3MPa) places optical-grade requirements on the protective film. GB618's technological breakthroughs in this field are reflected in:


Optical purity: The adhesive layer uses a solvent-free UV curing system, with total volatile organic compounds (TVOC) <50μg/g, avoiding optical contamination.


Thermal stability: Dimensional shrinkage at 90℃ is <0.1%, far lower than 6318B's 0.3%, ensuring the angular accuracy of the polarizer.


Release force stability: After 500 hot-pressing cycles, the release force fluctuation is <±8%, ensuring the stability of automated production.


Test data from a leading domestic eyeglass lens manufacturer shows that the yield rate of polarizers increased by 1.8% after adopting GB618, mainly attributed to the elimination of film wrinkles and residual adhesive contamination during the hot-pressing process.


6. Empirical Research on Market Substitution


6.1 Cost Structure Optimization


Although GB618 uses a more advanced TPE system in its raw material formulation, it achieves a reduction in overall cost through the following means:


Improved Process Efficiency: Reduced rework rate due to the absence of stoppage lines, saving 0.5 man-hours per shift per production line.


Reduced Scrap Rate: GB618 reduces scrap rate to 0.8%.


Shortened Supply Chain: Domestic supply cycle shortened from 6-8 weeks to 2 weeks, reducing inventory costs by 40%.


Comprehensive calculations show that the per-vehicle protection cost (BOM cost + quality cost) for OEMs using GB618 is approximately 12% lower than that of 6318B.


6.2 Supply Chain Security Value


Against the backdrop of geopolitical risks and trade barriers facing the global automotive industry, the localization of GB618 achieves independent control over key materials. Its production base has obtained IATF 16949 certification, establishing a vertically integrated system from PP copolymerization and TPE synthesis to precision coating, avoiding the supply chain vulnerability of 6318B, which relies on imported raw materials.


7. Conclusion and Outlook


The complete replacement of Sekisui 6318B by Jidong New Materials' GB618 represents a leap in materials science from "performance imitation" to "mechanism innovation." Through deep integration of molecular-level formulation design and multi-layer co-extrusion technology, GB618 achieves comprehensive superiority in key indicators such as acoustic performance, interface cleanliness, and optical purity while maintaining process compatibility. It has also established a technological moat in niche areas such as automotive metal parts, plastic part protection, and polarizer hot-pressing.


In the future, as the surface quality requirements of new energy vehicles continue to increase (such as integrated die-cast body and intelligent cockpit optical components), the GB618 technology platform can further evolve in the following directions:


1. Functional Integration: Develop conductive and thermally conductive protective films to meet electromagnetic shielding and thermal management needs.


2. Intelligentization: Embed pressure-sensitive or temperature-responsive materials to achieve visualized monitoring of the protection process.


3. Green Development: Adopt bio-based PP and recyclable TPE systems to align with carbon neutrality goals.


The successful implementation of GB618 proves that domestic substitution is not simply a matter of performance benchmarking, but rather a value reconstruction through a deep understanding of the pain points in end-process manufacturing and fundamental material innovation. This not only provides a guarantee for the security of China's automotive parts supply chain but also contributes Chinese solutions to the advancement of global automotive materials technology.