Suzhou Jidong New Material Technology Co., Ltd
Service Hotline:
0086 139 229 345 98
E-mail:13922934598@139.com
Online customer service
 Work Time
Mon to Fri :8:00-20:00
Sat to Sun :9:00-17:00
 Contact Details
手机:0086 139 229 345 98
邮箱:409639645@qq.com

Discussion on the requirements of protective film for semiconductor wafer glass

  60

Semiconductor wafer glass is the core foundational material for semiconductor products such as integrated circuits, optoelectronic devices, and microelectromechanical systems (MEMS). It has excellent transparency, insulation, thermal stability, and dimensional accuracy, and is widely used in key areas such as wafer substrates, packaging covers, and optical windows. With the continuous reduction of semiconductor process nodes, the size of wafer glass gradually increases and the thickness continues to decrease. Its surface is susceptible to scratches, wear, pollution and other damages. At the same time, during cutting, grinding, coating, bonding and other processing processes, it needs to withstand complex working conditions such as temperature changes, mechanical stress, chemical environment, etc., which puts more stringent requirements on the protective film used for surface protection.

The protective film is precisely adhered to the surface of the wafer glass to form a temporary protective barrier, which can effectively isolate external pollutants such as dust, metal particles, and water vapor, alleviate mechanical impact and friction damage during processing, suppress the risk of device breakdown caused by static electricity accumulation, and adapt to the special requirements of different processing techniques. After the process is completed, it can be peeled off without residue or damage. Currently, the rapid development of the semiconductor industry is driving the upgrading of wafer glass towards high purity, high flatness, ultra-thin, and large-sized directions. Traditional protective films are no longer able to meet the protection needs of high-end wafer glass, resulting in problems such as residual glue, scratches, and poor adaptability, which seriously affect the yield and reliability of semiconductor devices. Therefore, clarifying the core requirements of protective film for semiconductor wafer glass and developing high-performance and highly adaptable protective film materials have become important supports for the high-quality development of the semiconductor industry chain. This article discusses in detail the various requirements for the protective film required for semiconductor wafer glass, based on its characteristics and processing technology.

半导体晶元玻璃-2.jpg

Core characteristics and protection requirements of semiconductor wafer glass

The material characteristics and application scenarios of semiconductor wafer glass determine its core protection requirements for protective films, which is the basis for clarifying the requirements for protective films. Semiconductor wafer glass is often made of high-purity quartz glass, borosilicate glass and other materials, which have the following key characteristics: firstly, the surface flatness is extremely high, and the roughness is usually controlled at the nanometer level, without any small scratches, depressions or protrusions on the surface, otherwise it will affect the accuracy of subsequent coating, lithography and other processes; Secondly, it has excellent chemical stability, but still has a certain sensitivity to corrosive substances such as fluoride, strong acids and bases. At the same time, the surface is prone to adsorb pollutants such as dust and metal ions from the air, which can cause faults such as leakage and short circuits in semiconductor devices; Thirdly, the mechanical strength is relatively low, especially for ultra-thin wafer glass (thickness<100 μ m), which has weak impact resistance and wear resistance, and is prone to damage and edge breakage during processing and transportation; The fourth is excellent insulation, but it is prone to static electricity. The accumulation of static electricity can adsorb small particles and may also penetrate sensitive structures on the glass surface of the wafer; Fifth, the dimensional accuracy is extremely high. The dimensional deviation of large-sized wafer glass (such as 12 inches and above) needs to be controlled at the micrometer level, and the bonding of the protective film needs to avoid stress and prevent warping and deformation of the wafer glass.

Based on the above characteristics, the core protection requirements of semiconductor wafer glass for protective films can be summarized into four points: firstly, pollution protection, which prevents external pollutants such as dust, metal ions, water vapor, and organic matter from adhering to the surface of the wafer glass; The second is damage protection, to avoid mechanical friction, impact, compression, etc. during processing and transportation that may cause scratches, damages, or edge breakage on the surface of the wafer glass; The third is electrostatic protection, which suppresses the static electricity generated during the bonding and peeling process between the protective film and the wafer glass, avoiding electrostatic adsorption of pollutants or breakdown of device structures; The fourth is process adaptation, which adapts to the temperature, chemical environment and other requirements of different processing techniques such as cutting, grinding, coating, photolithography, bonding, etc., to ensure smooth process and no residue or damage after peeling. These protective requirements directly determine the specific requirements of the protective film in terms of physical properties, chemical properties, cleanliness, and process adaptability.

Core requirements for protective film of semiconductor wafer glass

2.1 Physical Performance Requirements

The physical properties of the protective film are the basis for achieving effective protection of wafer glass, directly affecting the protection effect and processing adaptability, mainly including thickness accuracy, flatness, mechanical strength, adhesive properties, and electrostatic performance.

Thickness accuracy and flatness are one of the core physical indicators of protective films. The surface flatness of semiconductor wafer glass is extremely high, and the protective film needs to be perfectly adhered to the wafer glass without bubbles or wrinkles. This requires excellent thickness uniformity of the protective film, with a thickness deviation controlled within ± 2 μ m, to avoid uneven thickness leading to loose adhesion, gas bubbles or stress, and thus causing warping and deformation of the wafer glass. At the same time, the surface flatness of the protective film should match the surface roughness of the wafer glass, with a roughness not exceeding 1/2 of the surface roughness of the wafer glass, to prevent protrusions on the surface of the protective film from scratching the surface of the wafer glass. In addition, the thickness of the protective film needs to be adapted according to the thickness of the wafer glass and the processing technology. For ultra-thin wafer glass, a thinner protective film should be selected to reduce the overall thickness after bonding and avoid affecting subsequent process operations; The protective film used for cutting and grinding processes needs to have a certain thickness to provide sufficient mechanical support and prevent damage to the wafer glass.

In terms of mechanical strength, the protective film needs to have good tensile, tear, and wear resistance. During the cutting, grinding, and other processing of wafer glass, the protective film needs to withstand a certain mechanical stress. If the tensile strength is insufficient, it is prone to fracture; If the tear resistance is poor, it will cause the protective film to break and lose its protective effect; If the wear resistance is poor, the surface of the protective film is prone to scratches, which can transfer to the surface of the wafer glass and cause damage. Usually, the tensile strength of the protective film should be ≥ 15MPa, the tear strength should be ≥ 50N/m, and the surface hardness should be moderate. It should have certain wear resistance but not be too hard to avoid scratching the wafer glass during the bonding and peeling process. For protective films used on ultra-thin wafer glass, good flexibility is also required, which can tightly adhere to the curved surface of the wafer glass (if any) during bonding, while avoiding excessive bonding stress.

Adhesive properties are the key performance of protective films, which directly affect the stability of bonding and the safety of peeling. It is necessary to achieve a balance between "firm bonding and residue free peeling". In the bonding stage, the protective film needs to have suitable adhesion, which can tightly adhere to the surface of the wafer glass without bubbles or warping. At the same time, the adhesion needs to be evenly distributed to avoid insufficient local adhesion causing weak bonding, or excessive local adhesion causing difficulty in peeling off. According to different processing techniques, the adhesion of the protective film needs to be precisely controlled: for protective films used for storage and transportation, the adhesion should be moderate (10-20g/in) to ensure a firm bond and no residue during peeling; The protective film used for cutting and grinding processes needs to have a high viscosity (40-100g/in) to provide sufficient fixing force, prevent displacement and scattering of wafer glass during processing, and reduce breakage during cutting; The protective film used for photolithography and coating processes needs to have low adhesion (5-10g/in) to avoid damaging sensitive structures or photoresist layers on the wafer glass surface during peeling. In addition, the adhesion of the protective film needs to have good stability, with a viscosity change of no more than 10% under different temperature and humidity environments, to avoid adhesion failure or residual peeling caused by environmental changes. It is worth noting that UV protective film needs to have high viscosity before UV irradiation, and the viscosity needs to decrease significantly after irradiation (to below 2-5g/in) to ensure that the chips do not scatter or have residual glue during picking up. At the same time, the UV reaction time needs to be fast to improve processing efficiency.

In terms of electrostatic performance, the protective film needs to have good anti-static ability to suppress the generation and accumulation of static electricity. Semiconductor wafer glass is prone to static electricity, which can adsorb pollutants such as small dust and metal particles in the air, and may also penetrate sensitive structures on the surface of the wafer glass, affecting the performance of semiconductor devices. Therefore, the protective film needs to have anti-static function, with surface resistance controlled within the range of 10 ⁶ -10 ⁹ Ω. The static voltage generated during the bonding and peeling process should be ≤ 500V to avoid static accumulation. In addition, the anti-static performance of the protective film needs to have durability, and it should not fail due to environmental changes during storage and processing. At the same time, the anti-static agent should not migrate to the surface of the wafer glass to avoid pollution.

2.2 Chemical performance requirements

Semiconductor wafer glass has low sensitivity to chemical substances, but the protective film may undergo chemical reactions with the wafer glass or release chemical substances during bonding, processing, and storage, causing pollution. Therefore, the protective film needs to have excellent chemical stability and low precipitation to meet the chemical protection requirements of the wafer glass.

Firstly, the protective film needs to have good chemical stability and not undergo chemical reactions with semiconductor wafer glass. The main component of wafer glass is silicon dioxide. The substrate and adhesive layer of the protective film should avoid containing corrosive substances such as fluoride, strong acid and alkali, otherwise they will react with the surface of the wafer glass, causing corrosion, discoloration, increased roughness and other problems, which will affect the subsequent process accuracy and device performance. At the same time, the protective film needs to be able to withstand the chemical environment during semiconductor processing, such as photoresist, developer solution in photolithography process, organic solvents, deionized water in cleaning process, etc., without dissolution, deformation, aging and other phenomena, ensuring the stability of the protective function. For example, the protective film used for wafer glass thinning and cutting processes needs to have good acid and alkali resistance, be able to withstand acid and alkali solutions that may come into contact during processing, and avoid problems such as adhesive layer detachment and substrate damage.

Secondly, the protective film needs to have low precipitation and not release any pollutants. If there are easily precipitated substances such as plasticizers, stabilizers, residual solvents, etc. in the substrate and adhesive layer of the protective film, these substances will migrate to the surface of the wafer glass, forming pollutants and causing faults such as leakage and short circuit in semiconductor devices. Therefore, the protective film needs to strictly control the precipitation content to ensure that there are no volatile organic compounds (VOCs), no siloxanes, and no metal ions (such as Na ⁺, K ⁺, etc.) precipitation. The metal ion content should be controlled at the ppb level to avoid affecting the electrical characteristics of CMOS and capacitor devices. At the same time, the adhesive layer of the protective film needs to have good stability, and there should be no residual adhesive after peeling. The residual adhesive rate should be controlled below 0.01%, otherwise the residual adhesive will adsorb pollutants or affect the accuracy of subsequent coating, photolithography and other processes. In addition, the protective film needs to avoid environmental pollutants such as heavy metals and harmful organic compounds, which comply with the environmental protection requirements of the semiconductor industry.

In addition, the protective film needs to have good temperature resistance and adapt to temperature changes during semiconductor processing. The processing technology of semiconductor wafer glass (such as coating, bonding, baking, etc.) usually needs to be carried out at a certain temperature, with a temperature range of -10 ℃~250 ℃. The temperature requirements for different processes vary: back grinding and bonding usually require 60-120 ℃, RDL process can reach 120-200 ℃, and laser and some temporary bonding/de bonding processes can even exceed 250 ℃. Therefore, the protective film needs to maintain stable physical and chemical properties within this temperature range, without softening, deformation, aging, decomposition, and other phenomena. At the same time, the adhesive bonding should not undergo significant changes to avoid the protective film falling off or residue due to temperature changes. For example, protective films used in high-temperature coating processes need to have high temperature resistance (≥ 200 ℃), not release harmful substances in high-temperature environments, and not react with wafer glass; The protective film used for low-temperature storage needs to have low-temperature resistance (≤ -10 ℃), without brittleness or fracture.

2.3 Cleanliness requirements

The surface cleanliness of semiconductor wafer glass directly determines the yield and reliability of semiconductor devices. Any small pollutants (such as dust, metal particles, organic matter, etc.) can cause device failures. Therefore, protective films need to have extremely high cleanliness, not become a source of pollution themselves, and effectively block external pollutants.

The cleanliness of protective film is mainly reflected in three aspects: firstly, it is free of pollutants. During the production process, the protective film needs to use a high cleanliness production environment (such as Class 100 or Class 1000 clean workshops), strictly control the purity of raw materials such as substrates and adhesive layers, and avoid impurities such as dust and metal particles in the raw materials. At the same time, during the production process, it is necessary to avoid defects such as scratches, stains, wrinkles, etc. on the surface of the protective film. The finished protective film needs to undergo strict cleanliness testing to ensure that there are no visible pollutants on the surface. The number of small particles (particle size ≥ 0.5 μ m) is ≤ 10 per square meter, and the number of metal particles (particle size ≥ 0.1 μ m) is ≤ 5 per square meter. Secondly, there should be no dust shedding, and the substrate and adhesive layer of the protective film should have good stability. During the bonding, peeling, and processing processes, there should be no dust shedding, fiber shedding, or other phenomena to prevent the shedding dust from adhering to the surface of the wafer glass and causing pollution. Thirdly, it has the ability to block pollutants, and the protective film needs to have good sealing properties. After bonding, it can tightly cover the surface of the wafer glass without gaps or bubbles, effectively blocking pollutants such as dust, water vapor, and metal ions in the external air, and preventing them from adhering to the surface of the wafer glass.

In addition, the packaging of the protective film also needs to meet the cleanliness requirements, using high cleanliness packaging materials (such as dust-free paper, dust-free plastic bags), and avoiding secondary pollution during the packaging process. The finished protective film needs to be sealed and stored in a clean, dry, and pollution-free environment to avoid contamination during storage. At the same time, the surface tension of the protective film should be uniform to avoid uneven surface tension leading to loose adhesion, the generation of bubbles, and the adsorption of pollutants. For high-end semiconductor wafer glass, the cleanliness of the protective film must comply with the SEMI F57-0301 standard and ISO 14644-1 certification requirements to ensure that it meets the production needs of high-end semiconductor devices.

2.4 Requirements for Process Adaptability

The processing flow of semiconductor wafer glass is complex, covering multiple process steps such as cutting, grinding, coating, photolithography, bonding, and cleaning. Different processes have different requirements for the protective film, so the protective film needs to have good process adaptability to meet the special needs of different processing processes and ensure the smooth progress of the process.

In the cutting process, the protective film needs to have good cutting adaptability, be able to tightly adhere to the surface of the wafer glass, provide sufficient support, prevent displacement, edge breakage, and damage of the wafer glass during the cutting process, and not generate a large amount of dust during the cutting process. The cutting edge should be free of residual glue and burrs, avoiding affecting the subsequent chip picking process. For the DBG process that undergoes post grinding after half cutting, the protective film should be able to effectively reduce adverse phenomena such as backside fragmentation, cracks, and chip edge cracking, ensuring the integrity of the grains during cutting without any grain loss. In addition, the protective film after cutting should be easy to peel off, with no residue or damage during peeling, and not affect the subsequent packaging of the chip.

In the grinding process, the protective film needs to have good wear resistance and impact resistance, able to withstand mechanical friction and impact during the grinding process, avoiding scratches on the surface of the wafer glass by grinding particles. At the same time, the protective film needs to have good sealing properties to prevent grinding liquid and grinding particles from entering between the protective film and the wafer glass, causing pollution or scratches. For the wafer back thinning process, the protective film needs to have good adhesion stability, effectively support ultra-thin wafer glass, reduce wafer warping and deformation caused by stress, and after the thinning process is completed, no residual peeling can be achieved through chemical treatment (such as alkaline solution treatment) or UV exposure to ensure that the thinned wafer surface is clean and undamaged. For example, temporary protective films prepared using photopolymerization liquid phase compositions have good fluidity, strong adhesion, and can uniformly cover the surface of wafers. After film formation, the surface flatness is good, and the degree of wafer warping after back grinding is small. After processing, they can be peeled off by NaOH alkaline solution without residue.

In the coating and lithography processes, the protective film needs to have good light transmittance (if used for front protection), with a light transmittance of ≥ 90%, without affecting the penetration of lithography light and the uniformity of the coating. At the same time, the surface of the protective film needs to have good flatness and cleanliness to avoid affecting the lithography accuracy and coating quality. In addition, in the photolithography process, the protective film should not react with the photoresist, and should not affect the coating, exposure, development, and other processes of the photoresist. After peeling, there should be no residual photoresist, and it should not affect the subsequent etching process. For high-end packaging processes such as RDL, the protective film needs to use a non silicon system to avoid silicone contamination, while also having low VOC and low metal ion characteristics to meet the high cleanliness requirements of the process.

In the bonding process, the protective film needs to have good resistance to high temperature and high pressure, be able to withstand high temperature (≥ 200 ℃) and high pressure during the bonding process, without softening, deformation, decomposition, and other phenomena, while not affecting the sealing and strength of the bonding. After bonding is completed, it can be left without residue or damage. In addition, the bonding of the protective film should avoid generating stress to prevent the wafer glass from warping and deforming during the bonding process, which may affect the bonding accuracy.

In addition to the above process, the protective film also needs to have good bonding and peeling convenience. During the bonding process, it can be quickly and evenly bonded without bubbles or wrinkles, and the bonding efficiency is high; During the peeling process, it can be manually or mechanically peeled with moderate peeling force (1-5N/25mm), uniform peeling speed, no residue or damage, no static electricity generated, and no impact on the subsequent processing of wafer glass. For UV type protective films, it is necessary to support low-temperature wafer backside adhesion. The UV exposure reaction time is fast (10-30 seconds), effectively improving work efficiency. At the same time, the adhesion decreases significantly after exposure, making it easy to pick up.


2.5 Environmental Protection and Safety Requirements

With the increasing global awareness of environmental protection and the demand for green development in the semiconductor industry, protective films for semiconductor wafer glass need to have good environmental and safety properties, comply with relevant environmental standards, and avoid harm to the environment and human health.

In terms of environmental protection, the protective film should use environmentally friendly raw materials to avoid the use of environmental pollutants such as heavy metals and harmful organic compounds (such as polycyclic aromatic hydrocarbons, formaldehyde, etc.). The raw materials should comply with international environmental standards such as RoHS and REACH. At the same time, the production process of protective film needs to be green and environmentally friendly, reducing the discharge of wastewater, exhaust gas, and waste residue, and reducing environmental pollution; After the protective film is discarded, it should be able to naturally degrade or recycle, reduce solid waste pollution, and avoid long-term environmental impact. For example, protective films prepared using solvent-free photopolymerization liquid phase compositions are non-volatile at room temperature, with minimal changes in physical properties and minimal environmental pollution, meeting the requirements of green production.

In terms of safety, the protective film needs to have good safety. During storage, transportation, and use, there should be no danger such as combustion or explosion, and no release of toxic or harmful gases to avoid harm to human health. At the same time, the adhesive material of the protective film should be non irritating to avoid adverse reactions such as allergies caused by contact with human skin; The packaging of protective film should have good safety to avoid packaging damage that may cause contamination or danger to the protective film. In addition, the protective film needs to have a certain level of storage stability. Under the specified storage conditions (temperature 10-30 ℃, humidity 40% -60%), the storage period should not be less than 6 months, and there should be no changes in viscosity, aging, or damage during storage to ensure stable performance.

Existing problems and development trends in the application of protective films

3.1 Existing Problems

Although there has been some progress in the research and application of protective films for semiconductor wafer glass, there are still many problems in the high-end semiconductor industry that cannot meet the protection needs of high-purity, ultra-thin, and large-sized wafer glass. One issue is the insufficient precision of adhesive control. Some protective films have problems such as weak adhesion and residual adhesive during peeling, especially for ultra-thin wafer glass protective films. High adhesion can easily lead to peeling damage, while low adhesion can easily cause bonding failure; Secondly, the chemical stability and temperature resistance need to be improved. In high temperature and strong chemical environments, some protective films may soften, decompose, release harmful substances, or react with wafer glass, causing pollution and damage; Thirdly, the cleanliness is difficult to meet high-end demands, and some protective films have problems such as small particles and dust shedding, which become a source of contamination for wafer glass and affect the yield of semiconductor devices; Fourthly, the adaptability of the process is poor, and a single protective film is difficult to adapt to multiple processing techniques, requiring frequent replacement of the protective film, which increases production costs and processing complexity; The fifth issue is that high-end protective films rely on imports. Domestic protective films have a gap with international advanced levels in terms of material purity, performance stability, and process adaptability, making it difficult to meet the protection needs of high-end semiconductor wafer glass. In addition, the existing protective film also has problems such as excessive thickness deviation, uneven thermal shrinkage rate, and poor electrostatic control effect, which limit its application in high-end semiconductor processes.

3.2 Development Trends

Based on the development direction and protection requirements of semiconductor wafer glass, protective films for semiconductor wafer glass will develop towards high performance, high adaptability, green environmental protection, and integration in the future. One is high-performance, with a focus on improving the thickness accuracy, flatness, viscosity control accuracy, chemical stability, temperature resistance, and cleanliness of protective films. We will develop high-end protective films that are adhesive free, dust-free, anti-static, and high-temperature resistant to meet the protection needs of ultra-thin, large-sized, and high-purity wafer glass; The second is high adaptability, developing multifunctional integrated protective films that can adapt to multiple processing techniques such as cutting, grinding, coating, and photolithography, reducing the number of protective film replacements and improving processing efficiency. At the same time, according to different process requirements, the performance parameters of the protective film can be accurately controlled to achieve "one film for multiple uses"; The third is green environmental protection, further optimizing raw materials and production processes, using biodegradable and recyclable environmentally friendly raw materials, reducing pollutant emissions in the production process, promoting the green development of the protective film industry, and complying with global environmental trends; The fourth is localization substitution, increasing research and development investment in domestic protective films, breaking through core technology bottlenecks, improving material purity, performance stability, and process adaptability, narrowing the gap with international advanced levels, achieving localization substitution of high-end protective films, and reducing the external dependence of the semiconductor industry chain; The fifth is intelligence. Combining with the trend of intelligent semiconductor processing, we will develop protective films with intelligent monitoring functions, which can monitor the bonding status, pollution situation, static electricity accumulation, etc. in real time, provide timely feedback on abnormal information, and improve the reliability and intelligence level of protection. In addition, new types of protective films such as photopolymerization and chemical exfoliation will become research and development hotspots. These protective films have the advantages of convenient exfoliation, no residue, and strong adaptability, which can effectively solve the problems of residual glue and damage in existing protective films and meet the needs of high-end semiconductor processes. At the same time, non silicon protective films will rapidly develop to meet the stringent requirements of advanced processes for low VOC, low precipitation, and no siloxane pollution.

4 Conclusion

As the core substrate of semiconductor devices, the surface integrity, cleanliness, and structural stability of semiconductor wafer glass directly determine the yield and reliability of the devices. The protective film, as a key auxiliary material for its full process protection, needs to meet strict requirements in various aspects. This study shows that the core requirements for protective films on semiconductor wafer glass are mainly reflected in five aspects: physical properties, chemical properties, cleanliness, process adaptability, and environmental safety. In terms of physical properties, it needs to have excellent thickness accuracy, flatness, mechanical strength, adhesive properties, and electrostatic properties to achieve effective protection and convenient peeling; In terms of chemical properties, it is necessary to have good chemical stability, low precipitation, and temperature resistance to avoid reacting with wafer glass or causing pollution; In terms of cleanliness, it is necessary to have extremely high self cleanliness and pollutant barrier ability, so as not to become a source of pollution; In terms of process adaptability, it is necessary to meet the special requirements of different processing techniques such as cutting, grinding, and coating, and achieve multi process adaptation; In terms of environmental safety, it is necessary to comply with environmental standards and avoid harm to the environment and human health.

Currently, the rapid development of the semiconductor industry is driving the upgrade of wafer glass towards high purity, ultra-thin, and large-sized. Traditional protective films are no longer able to meet high-end protection needs, and there are problems such as insufficient viscosity control accuracy, poor chemical stability, and inadequate cleanliness. In the future, we need to focus on the protection needs of wafer glass, increase research and development investment in high-performance protective films, break through core technology bottlenecks, improve the performance and adaptability of protective films, promote the development of protective films towards high performance, high adaptability, green environmental protection, and localization, and provide support for the high-quality development of the semiconductor industry chain. At the same time, it is necessary to strengthen the research and development of performance testing technology for protective films, establish comprehensive testing standards, ensure that the quality of protective films meets the protection requirements of semiconductor wafer glass, and further improve the yield and reliability of semiconductor devices.

成功打破日韩品牌对光学保护膜领域的垄断.jpg